Wafer Bonder
Jump to navigation
Jump to search
|
Description
The SB6L wafer bonder applies force and heat to the back side of two wafers in a vacuum chamber in order to bond them face to face. An automatic recipe can be created with control over bonding pressure, temperature, and chamber pressure as well as ramp & duration of any process step. Since heat and temperature can be controlled separately, temperature-sensitive materials such as polymers may be bonded.
Applications
- MEMS & Microelectronics Fabrication
Resources
SOPs
Manufacturer Manuals
- NP12 User Manual - The SUSS NP 12™ Plasma Activation System User Manual
- Suss Micro Tec Process Manual -The Wafer Bonding Process Manual contains information on the different types of substrate bonding applications.