Tube Furnaces for Wet & Dry Processing
Jump to navigation
Jump to search
|
Description
The system is designed for processing up to one-hundred, 150 mm (6") silicon or sapphire wafers per tube and can accommodate smaller sample sizes also. Tube 1 is designated for wet & dry oxidation using a flask evaporator. Tube 2 is designated for dry oxidation and annealing.
Applications
- Dry & Wet oxidation
- Annealing
Allowed Materials
- Silicon or sapphire that is completely free of metal or organic contamination
- Recommended to have undergone a standard RCA clean or similar beforehand
- No other sample material allowed
- No metal or organic contamination
- Wafers must not have been contacted by metal tweezers, etc. without appropriate cleaning to remove metal contamination
Gas List
- Nitrogen
- Oxygen
- Water Vapor (Tube 1)