EBPG 5200: 100 kV Electron Beam Lithography: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
mNo edit summary |
||
| Line 5: | Line 5: | ||
|ImageTwo = EBPG-5200-Instrument-Image.jpg | |ImageTwo = EBPG-5200-Instrument-Image.jpg | ||
|InstrumentType = [[Equipment_List#Lithography|Lithography]] | |InstrumentType = [[Equipment_List#Lithography|Lithography]] | ||
|RoomLocation = | |RoomLocation = B233C Steele | ||
|LabPhone = 626-395-1531 | |LabPhone = 626-395-1531 /1540 | ||
|PrimaryStaff = [[Guy A. DeRose, PhD]] | |PrimaryStaff = [[Guy A. DeRose, PhD]] | ||
|StaffEmail = derose@caltech.edu | |StaffEmail = derose@caltech.edu | ||
Revision as of 17:47, 30 April 2019
|
Description
The Raith EBPG 5200 is a direct-write Electron Beam Pattern Generator that is used to pattern large areas by high resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation.
Type1 Applications
- Application1
- Application2
- Application3
Type2 Applications
- Application1
- Application2
- Application3
Resources
SOPs & Troubleshooting
Video Tutorials
Graphical Handouts
Presentations
Manufacturer Manuals
Specifications
Manufacturer Specifications
Specifications
- Voltage Range: 20, 50 or 100 kV
- Current Range: 50 pA - >200 nA
- Main Field size: Up to 1mm x 1mm
- Main Field resolution: 20 bit
- Maximum writing frequency: 100 MHz
- Aperture Sizes: 200um, 300um, 400um
- etc.
Mode 2 Specifications
- Voltage Range: 20, 50 or 100 kV
- Current Range: 50 pA - >200 nA
- etc.