Description
The Solaris 150 is a manual loading Rapid Thermal Processor system that can process up to 6 inch substrates. The system is designed for silicon implant annealing and monitoring and compound semiconductor implant activation and ohmic alloying.
Applications
- Temperature range from room temperature to 1200 degrees C.
- Processing gasses available:
- Nitrogen
- Argon
- Forming Gas (5% H2 in N2)