CNI-PV 2.1: Nano Imprint Lithography: Difference between revisions
Jump to navigation
Jump to search
(Created page with "{{instrument|{{PAGENAME}} |InstrumentName = NIL Technology CNI-PV 2.1 Nano Imprint Lithography System |HeaderColor = #F5A81C |ImageResearch = Research.jpg |ImageInstrument = I...") |
|||
| Line 47: | Line 47: | ||
== Specifications == | == Specifications == | ||
* Thermal NanoImprint: Up to 240°C with 150x150 mm substrate | * Thermal NanoImprint: Up to 240°C with 150x150 mm substrate | ||
* UV | * UV NanoImprint up to 200 mm wafers | ||
<br> | <br> | ||
<br> | <br> | ||
== Related Instrumentation in the KNI == | == Related Instrumentation in the KNI == | ||
===== Electron Beam Lithography ===== | ===== Electron Beam Lithography ===== | ||
Revision as of 23:30, 28 September 2020
|
Description
The NIL Technology CNI-PV 2.1 Nano Imprint Lithography System is a lithography tool that is used to enable nanoscale printing by thermal or UV exposure of photoresist with an imprint stamp. Vacuum in the imprint chamber is enabled down to 1 micron, and thermal imprint of up to 240°C is available. The system is compatible with UV-cured resists, and has an integral UV light source for those processes. It allows up to 200 mm diameter substrates with UV, or up to 150x150 mm substrates with thermal processing.
Operational Applications
- Thermal Nano Imprint Lithography
- UV Nano Imprint Lithography
Scientific / Technical Applications
- Nanophotonics
- Nano-optics
- Waveguides
Resources
Equipment Data
General SOPs
Training Materials
Sample Prep and Writing SOPs
Advanced Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals
Specifications
- Thermal NanoImprint: Up to 240°C with 150x150 mm substrate
- UV NanoImprint up to 200 mm wafers
Related Instrumentation in the KNI
Electron Beam Lithography
- EBPG 5200: 100 kV Electron Beam Lithography
- EBPG 5000+: 100 kV Electron Beam Lithography
- Quanta 200F: SEM with 1-30 kV Electron Beam Lithography