* [https://caltech.box.com/s/nwuxjbfm0fp0lb4k12albsr3zbnqk9po Bi-Layer PMMA Resist Spinning Recipe]
* [https://caltech.box.com/s/nwuxjbfm0fp0lb4k12albsr3zbnqk9po Bi-Layer PMMA Resist Spinning Recipe]
* [https://caltech.box.com/s/db1hiyshj5vovhwr3mvxn0glzn0xnabp Recipe to prepare PMMA developer (MIBK:IPA 1:3)]
* [https://caltech.box.com/s/2pumpha7ywa8zenvfzjxlggglvm4u3h5 MAN Resist Data Sheet]
* [https://caltech.box.com/s/2pumpha7ywa8zenvfzjxlggglvm4u3h5 MAN Resist Data Sheet]
* [https://caltech.box.com/s/lw2h56h0lqabwo82yofu52dqgi61gcp9 PMMA Resist Data Sheet]
* [https://caltech.box.com/s/lw2h56h0lqabwo82yofu52dqgi61gcp9 PMMA Resist Data Sheet]

Revision as of 23:34, 18 August 2020

EBPG 5200
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5200

Description

The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

Equipment Data
General SOPs
Training Materials
Sample Prep and Writing SOPs
Advanced Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 200 μm, 300 μm, 400 μm