ICP-RIE: Dielectric Etcher: Difference between revisions
Jump to navigation
Jump to search
| Line 53: | Line 53: | ||
* [https://caltech.box.com/s/tfieodeis71aligdpgp3g13kuceefnh0 Oxford Plasmalab System 100 Dielectric Etcher Manual] | * [https://caltech.box.com/s/tfieodeis71aligdpgp3g13kuceefnh0 Oxford Plasmalab System 100 Dielectric Etcher Manual] | ||
* [https://caltech.box.com/s/juzfel0sy2fv6y3d1zcul8lc3z6ipha4 Edwards Pyrophoric Conditioning System Manual] | * [https://caltech.box.com/s/juzfel0sy2fv6y3d1zcul8lc3z6ipha4 Edwards Pyrophoric Conditioning System Manual] | ||
* [https://caltech.box.com/s/gclvux5tu28rpssvwncx5sm518uhmebl Edwards QDP 80 dry vacuum pump Manual] | |||
== Specifications == | == Specifications == | ||
Revision as of 21:03, 22 May 2019
|
Description
The Dielectric Inductively Coupled Plasma - Reactive Ion Etch (ICP-RIE) is an Oxford Instruments Plasma Technology Plasmalab System 100 ICP-RIE 380 system that is optimized for silicon etching. This system is configured for silicon etching with "pseudoBosch" C4F8 and SF6 gases, and cryogenic silicon etch with SF6 and O2. The silicon ICP-RIE has a variable temperature stage (-150 to 400 °C). This system supports wafer sizes up to 6 inches, and provides accurate deep etching capabilities for silicon and "silicon-like" samples only.
Applications
- Cryogenic etch of silicon
- pseudo-Bosch of silicon
Allowed material in Dielectric Etch System
- Si, SixNy, SiO2
- PMMA/ZEP/SPR/AZ/maN resists, SiOx/Al2O3 hard masks
- No metals
Dielectric Etcher Gas List
- SF6
- C4F8
- O2
- Ar
- N2
- CHF3
- N2O
- NH3
Resources
SOPs & Troubleshooting
- SOP Type (Short Version | Long Version)
- Etcher toxic gas handling SOP
- Power Up Oxford ICP-RIE SOP
- Gas Status Board SOP
- Troubleshooting Guide
Process Documents
Manufacturer Manuals
- Oxford Plasmalab System 100 Dielectric Etcher Manual
- Edwards Pyrophoric Conditioning System Manual
- Edwards QDP 80 dry vacuum pump Manual
Specifications
Manufacturer Specifications
System Features
- Universal base console which houses the electronic sub systems, control units, pneumatics, and turbomolecular pump
- PC 2000 Operating system
- ICP process chamber with 200mm pumping port, view port and end-point-detection ports for optical emission spectrometer and laser interferometer
- Variable height 240mm Cryo RIE electrode
- Parameter ramping software (Not Bosch)
- 100-mTorr, temperature-stabilized capacitance manometer for process control with an active penning gauge for base pressure measurement
- 200mm pumping port is fitted with a 200mm variable gate valve for chamber isolation and process pressure control
- Twelve line gas pod with 7 non-toxic and 3 toxic digital mass-flow-controlled gas lines
- Chamber Gas ring, with split gas manifold
- Alcatel 1300 l/s MAGLEV turbo pump
- Single-wafer automatic insertion load lock with soft pump option
System Specifications
- Chamber wall heating 80 deg C
- Cryo table range -140 to 400 deg C
- ICP 380mm remote high-density plasma source with 5kW RF generator and automatic matching unit close-coupled to the source.
- Substrate bias control by 30 / 300W RIE source
- Helium back-side wafer cooling