Usage Rates: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Created page with "This page will provide a list of the current instrument hourly rates and monthly cleanroom fee."
 
No edit summary
Line 1: Line 1:
This page will provide a list of the current instrument hourly rates and monthly cleanroom fee.
== Equipment Hourly Rates ==
{| class="wikitable" style="width: 75%;"
|-
!scope="col" style="text-align:left; width: 40%"| Equipment Name
!scope="col" style="text-align:center; width: 20%"| Caltech Rate
!scope="col" style="text-align:center; width: 20%"| JPL/Non-Caltech Acad/Govt Rate
!scope="col" style="text-align:center; width: 20%" | Corporate Rate
{{UsageRateTableItem|
|EquipmentName = AJA Chalcogenide Sputter
|CaltechRate = 64.00
|JPLNonCaltechAcadGovtRate = 97.67
|CorporateRate = 122.23
}}
{{UsageRateTableItem|
|EquipmentName = AJA Dielectric Sputter
|CaltechRate = 64.00
|JPLNonCaltechAcadGovtRate = 97.67
|CorporateRate = 122.23
}}
|}

Revision as of 18:55, 23 April 2019

Equipment Hourly Rates

Equipment Name Caltech Rate JPL/Non-Caltech Acad/Govt Rate Corporate Rate
AJA Chalcogenide Sputter
{{{EquipmentCategory}}}
$64.00
$97.67
$122.23
AJA Dielectric Sputter
{{{EquipmentCategory}}}
$64.00
$97.67
$122.23