ICP-RIE: Dielectric Etcher: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Nathslee (talk | contribs)
Derose (talk | contribs)
Line 48: Line 48:
* [https://caltech.box.com/s/daa9zeonjqphc8v963mi3lojo8me0u9j Cryo-Si Etch]
* [https://caltech.box.com/s/daa9zeonjqphc8v963mi3lojo8me0u9j Cryo-Si Etch]
* [https://caltech.box.com/s/ymt2wqtkkjwcyw5c71f2adm2a1u041zn Etch chamber cleaning recipes]
* [https://caltech.box.com/s/ymt2wqtkkjwcyw5c71f2adm2a1u041zn Etch chamber cleaning recipes]
===== Review Articles =====
* [https://caltech.box.com/s/3fnc4a7qeyr1up6kth599j7ojybka2vb Guidelines for Etching Silicon MEMS Structures]
* [https://caltech.box.com/s/j61w7vr4f8cdjr64jrnz1t37oizdhl7f Etch rates for MEMS Processing - Part I]
* [https://caltech.box.com/s/ls0jl268j4at6z39g6kv8wivevpq80eh Etch Rates for MEMS Processing - Part II]
* [https://caltech.box.com/s/cetpre7d66gssbhtaicnhtovyo6ngzjv Dry Etching of Electronic Oxides, Polymers, and Semiconductors]
* [https://caltech.box.com/s/pauf384duhejuwzfwan71eam7nkvdrxw Alumina etch masks for fabrication of high-aspect-ratio silicon micropillars and nanopillars]
* [https://caltech.box.com/s/q42u5q46nmx2hm53szub556kwcrc0oih David Henry's thesis on dry etching in the KNI's tools]


===== Manufacturer Manuals =====
===== Manufacturer Manuals =====
* [https://caltech.box.com/s/tfieodeis71aligdpgp3g13kuceefnh0 Oxford Plasmalab System 100 Dielectric Etcher Manual]
* [https://labrunr.caltech.edu/machinefiles/124/System%20Manual%20for%20Caltech%2094-219846_a.pdf Oxford Plasmalab System 100 Dielectric Etcher Manual] (<i>login to LabRunr required</i>)
* [https://caltech.box.com/s/juzfel0sy2fv6y3d1zcul8lc3z6ipha4 Edwards Pyrophoric Conditioning System Manual]
* [https://caltech.box.com/s/juzfel0sy2fv6y3d1zcul8lc3z6ipha4 Edwards Pyrophoric Conditioning System Manual]
* [https://caltech.box.com/s/gclvux5tu28rpssvwncx5sm518uhmebl Edwards QDP 80 dry vacuum pump Manual]
* [https://caltech.box.com/s/gclvux5tu28rpssvwncx5sm518uhmebl Edwards QDP 80 dry vacuum pump Manual]

Revision as of 17:22, 29 May 2019

Dielectric Etcher
Instrument Type Etching
Techniques Dielectric Material Etching
Staff Manager Nathan S. Lee
Staff Email nathslee@caltech.edu
Staff Phone 626-395-1319
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235 Steele
Lab Phone 626-395-1532
Manufacturer Oxford Instruments
Model Plasmalab System 100

Description

The Dielectric inductively-coupled plasma reactive-ion etcher (ICP-RIE) is an Oxford Instruments Plasma Technology Plasmalab System 100 ICP-RIE 380 system that is optimized for silicon etching. This system is configured for silicon etching with "pseudoBosch" C4F8 and SF6 gases, and cryogenic silicon etch with SF6 and O2. The silicon ICP-RIE has a variable temperature stage (-150 to 400 °C). This system supports wafer sizes up to 6 inches, and provides accurate deep etching capabilities for silicon and "silicon-like" samples only.

Applications
  • Cryogenic etch of silicon
  • pseudo-Bosch of silicon
Allowed material in Dielectric Etch System
  • Si, SixNy, Ge
  • PMMA/ZEP/SPR/AZ/maN resists, SiOx/Al2O3 hard masks
  • No metals
Dielectric Etcher Gas List
  • SF6
  • C4F8
  • O2
  • Ar
  • N2
  • CHF3
  • N2O
  • NH3

Resources

SOPs & Troubleshooting
Process Documents
Review Articles
Manufacturer Manuals

Specifications

Manufacturer Specifications
System Features
  • Universal base console which houses the electronic sub systems, control units, pneumatics, and turbomolecular pump
  • PC 2000 Operating system
  • ICP process chamber with 200 mm pumping port, view port and end-point-detection ports for optical emission spectrometer and laser interferometer
  • Variable height 240 mm Cryo RIE electrode
  • Parameter ramping software (Not Bosch)
  • 100-mTorr, temperature-stabilized capacitance manometer for process control with an active penning gauge for base pressure measurement
  • 200 mm pumping port is fitted with a 200mm variable gate valve for chamber isolation and process pressure control
  • Twelve line gas pod with 7 non-toxic and 3 toxic digital mass-flow-controlled gas lines
  • Chamber Gas ring, with split gas manifold
  • Alcatel 1300 l/s MAGLEV turbo pump
  • Single-wafer automatic insertion load lock with soft pump option
System Specifications
  • Chamber wall heating 80 °C
  • Cryo table range -140 to 400 °C
  • ICP 380 mm remote high-density plasma source with 5 kW RF generator and automatic matching unit close-coupled to the source.
  • Substrate bias control by 30 / 300 W RIE source
  • Helium back-side wafer cooling