For non-conductive specimens that cannot be effectively SEM or FIB-imaged with some combination of low voltage, low current, zero detector bias and scanning filters, depositing a thin (e.g. 2-10 nm), conductive layer of carbon on the surface can help. This carbon evaporator produces amorphous, conductive films, the morphology of which is not detectable in an SEM or FIB image. After imaging is complete, the carbon can be gently removed with an O<sub>2</sub> plasma using, for example, the lab's [[Tergeo Plus ICP- & CCP-RIE: Oxygen & Argon Plasma Cleaner | Tergeo Plus Plasma Cleaner]]. | For non-conductive specimens that cannot be effectively SEM- or FIB-imaged with some combination of low voltage, low current, zero detector bias, and scanning filters, depositing a thin (e.g. 2-10 nm), conductive layer of carbon on the surface can help. This carbon evaporator produces amorphous, conductive films, the morphology of which is not detectable in an SEM or FIB image. After imaging is complete, the carbon can be gently removed with an O<sub>2</sub> plasma using, for example, the lab's [[Tergeo Plus ICP- & CCP-RIE: Oxygen & Argon Plasma Cleaner | Tergeo Plus Plasma Cleaner]]. | ||
===== Applications ===== | ===== Applications ===== | ||
* Coat material surface to make sample conductive for use in an SEM or FIB | * Coat material surface to make sample conductive for use in an SEM or FIB | ||
* Coat resist surface to make sample conductive for use with e-beam lithography | * Coat resist surface to make sample conductive for use with e-beam lithography | ||
* Apply carbon to a specimen or device for any other fabrication use | * Apply carbon to a specimen or device for any other fabrication use | ||
| Line 26: | Line 26: | ||
[[Image:Carbon-Evaporator-Source-Thread.jpg|thumb|top|upright=0.9|The Carbon Evaporator source needs to be periodically disconnected from the instrument by the user so that the carbon thread can be changed; see the SOP and notes in the SOP section on this page for instructions on how to change the thread]] | [[Image:Carbon-Evaporator-Source-Thread.jpg|thumb|top|upright=0.9|The Carbon Evaporator source needs to be periodically disconnected from the instrument by the user so that the carbon thread can be changed; see the SOP and notes in the SOP section on this page for instructions on how to change the thread]] | ||
===== SOP & Troubleshooting ===== | ===== SOP & Troubleshooting ===== | ||
* [https://caltech.box.com/s/1l8kxgkiti1kgmvysl2tpu68r1desi8m SOP & | * [https://caltech.box.com/s/1l8kxgkiti1kgmvysl2tpu68r1desi8m SOP & Troubleshooting Guide] | ||
* The procedure to install a new carbon thread can be found on [https://www.manualslib.com/manual/1525180/Leica-Em-Ace600.html?page=43#manual Page 39 of the Operating Manual] | * The procedure to install a new carbon thread can be found on [https://www.manualslib.com/manual/1525180/Leica-Em-Ace600.html?page=43#manual Page 39 of the Operating Manual] | ||
** Note: always install as a "double thread," i.e. double the thread back over itself before installing – a thread length that is approximately twice the length of the evaporator's door width is long enough to double over and install. | ** Note: always install as a "double thread," i.e. double the thread back over itself before installing – a thread length that is approximately twice the length of the evaporator's door width is long enough to double over and install. | ||
Revision as of 19:58, 27 May 2019
|
Description
For non-conductive specimens that cannot be effectively SEM- or FIB-imaged with some combination of low voltage, low current, zero detector bias, and scanning filters, depositing a thin (e.g. 2-10 nm), conductive layer of carbon on the surface can help. This carbon evaporator produces amorphous, conductive films, the morphology of which is not detectable in an SEM or FIB image. After imaging is complete, the carbon can be gently removed with an O2 plasma using, for example, the lab's Tergeo Plus Plasma Cleaner.
Applications
- Coat material surface to make sample conductive for use in an SEM or FIB
- Coat resist surface to make sample conductive for use with e-beam lithography
- Apply carbon to a specimen or device for any other fabrication use
Resources

SOP & Troubleshooting
- SOP & Troubleshooting Guide
- The procedure to install a new carbon thread can be found on Page 39 of the Operating Manual
- Note: always install as a "double thread," i.e. double the thread back over itself before installing – a thread length that is approximately twice the length of the evaporator's door width is long enough to double over and install.
Video
Technical Notes
Manufacturer Manual
Specifications
Manufacturer Specifications
Carbon Evaporation Specifications
- Average Deposition Rate: ~1 nm per pulse, when using a double thread (i.e. a thread that is doubled over on itself; see notes in SOP section above)
- Monitor deposition thickness using the quartz crystal thickness monitor, or simply program the number of pulses that you want