EBPG 5200: 100 kV Electron Beam Lithography: Difference between revisions
Jump to navigation
Jump to search
| Line 41: | Line 41: | ||
* [https://caltech.box.com/s/55zji9vfs8kuxl0aye1sw1iy8xi0rd9c Information Archive Beam] | * [https://caltech.box.com/s/55zji9vfs8kuxl0aye1sw1iy8xi0rd9c Information Archive Beam] | ||
* [https://caltech.box.com/s/afdyjxjo54l1v2ukubon5ntin73aflc1 Lindgren MACS SOP] | * [https://caltech.box.com/s/afdyjxjo54l1v2ukubon5ntin73aflc1 Lindgren MACS SOP] | ||
* [https://caltech.box.com/s/pol1ceg2sbjsmbb6b5vtsw641hwj5r2l SAEHT not initialized] | * [https://caltech.box.com/s/pol1ceg2sbjsmbb6b5vtsw641hwj5r2l SAEHT not initialized SOP] | ||
* [https://caltech.box.com/s/tf87blqopht0y51hy4agn2fsfjh7wot9 EBPG Emergency air cylinder SOP] | * [https://caltech.box.com/s/tf87blqopht0y51hy4agn2fsfjh7wot9 EBPG Emergency air cylinder SOP] | ||
* [https://caltech.box.com/s/pol1ceg2sbjsmbb6b5vtsw641hwj5r2l EBPG SAEHT no route to host recovery ] | * [https://caltech.box.com/s/pol1ceg2sbjsmbb6b5vtsw641hwj5r2l EBPG SAEHT no route to host recovery SOP] | ||
* [https://caltech.box.com/s/1fe4803rl38fa7a7w50r77c4nf64818l EBPG hotbox slave communications fault recovery SOP] | |||
===== Video Tutorials ===== | ===== Video Tutorials ===== | ||
Revision as of 04:27, 7 May 2019
|
Description
The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation.
Opertional Applications
- Non-aligned electron beam lithography
- Aligned (AKA direct-write) electron beam lithography
Scientific / technical Applications
- Nanophotonics
- Nano-optics
- Waveguides
Resources
SOPs & Troubleshooting
- EBPG SOP Type (Short Version | Long Version)
- EBPG reservation and use policy
Sample Prep and Writing SOPs
- EBPG High Resolution Mode SOP
- EBPG 5200 Piece part prep SOP
- EBPG Marker definition Procedure
- EBPG JOY Marker Procedure
- EBPG Disable marker height check SOP
- EBPG Remote Access SOP
Troubleshooting SOPs
- Troubleshooting Guide
- Information Archive Beam
- Lindgren MACS SOP
- SAEHT not initialized SOP
- EBPG Emergency air cylinder SOP
- EBPG SAEHT no route to host recovery SOP
- EBPG hotbox slave communications fault recovery SOP
Video Tutorials
Graphical Handouts
Presentations
Manufacturer Manuals
Specifications
Manufacturer Specifications
Specifications
- Voltage Range: 20, 50 or 100 kV
- Current Range: 50 pA - >200 nA
- Main Field size: Up to 1mm x 1mm
- Main Field resolution: 20 bit
- Maximum writing frequency: 100 MHz
- Aperture Sizes: 200um, 300um, 400um