III-V Etcher and Atomic Layer Etching (ALE): Oxford Instruments PlasmaPro 100 Cobra 300 ICP-RIE with ALE: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Kmmckenz (talk | contribs)
Kmmckenz (talk | contribs)
 
(8 intermediate revisions by the same user not shown)
Line 2: Line 2:
|InstrumentName = Cobra III-V Etcher with ALE
|InstrumentName = Cobra III-V Etcher with ALE
|HeaderColor = #FFE2B9
|HeaderColor = #FFE2B9
|ImageOne = ICP-RIE_III-V,Metal,Si-Etcher.jpg
|ImageOne = Oxford_Cobra_1.jpg
|ImageTwo =  
|ImageTwo =  
|InstrumentType = [[Equipment_List#Etching|Etching]]
|InstrumentType = [[Equipment_List#Etching|Etching]]
Line 39: Line 39:
== Resources ==
== Resources ==
===== SOPs & Troubleshooting =====
===== SOPs & Troubleshooting =====
* General Use SOP
* [https://caltech.box.com/s/4plzcvkt78lnrn73c9kneopbkemrrrq7 Cobra Etcher SOP]
* [https://caltech.box.com/s/681uz0b8zsv6ivy43a5ggsoydp5zlyza Oxfords reservation and use policy]
* [https://caltech.box.com/s/681uz0b8zsv6ivy43a5ggsoydp5zlyza Oxfords reservation and use policy]
* Etcher toxic gas handling SOP
* Power Up Oxford ICP-RIE SOP


===== Process Documents =====
===== Process Documents =====
Line 62: Line 60:


===== Manufacturer Manuals =====
===== Manufacturer Manuals =====
* [https://labrunr.caltech.edu/machinefiles/126/System%20Manual%20for%20Caltech%2094-219845.pdf Oxford III-V Metal Etcher System Manual] (<i>login to LabRunr required</i>)
* [https://caltech.box.com/s/r2d8bk8mrtxa2qf0bwamuxn43cpjml4f PTIQ User Manual]
* [https://caltech.box.com/s/gclvux5tu28rpssvwncx5sm518uhmebl Edwards QDP 80 dry vacuum pump Manual]


== Specifications ==
== Specifications ==
===== Manufacturer Specifications =====
* [https://caltech.box.com/s/f8f1fx1ffz4ql71suxsvrw0p20b2inp5 Manufacturer Data Sheet]
===== System Features =====
===== System Features =====
* Process module frame and separate control rack that house the electronic sub systems, control units, pneumatics, and turbomolecular pump
* Process module frame and separate control rack that house the electronic sub systems, control units, pneumatics, and turbomolecular pump
* PTiQ operating system
* PTIQ operating system
* ICP process chamber with 200 mm pumping port, view port and end-point-detection ports for optical emission spectrometer and laser interferometer
* ICP process chamber with 200 mm pumping port, view port and end-point-detection port
* 240 mm Cryo RIE electrode
* 240 mm Cryo RIE electrode
* 100-mTorr, temperature-stabilized capacitance manometer for process control with an active penning gauge for base pressure measurement
* 100-mTorr, temperature-stabilized capacitance manometer for process control with an active penning gauge for base pressure measurement
Line 93: Line 87:
* [https://lab.kni.caltech.edu/ICP-RIE:_Dielectric_Etcher Oxford Dielectric ICP-RIE]
* [https://lab.kni.caltech.edu/ICP-RIE:_Dielectric_Etcher Oxford Dielectric ICP-RIE]
* [https://lab.kni.caltech.edu/DRIE:_Bosch_%26_Cryo_ICP-RIE_for_Silicon Oxford DRIE ICP-RIE]
* [https://lab.kni.caltech.edu/DRIE:_Bosch_%26_Cryo_ICP-RIE_for_Silicon Oxford DRIE ICP-RIE]
* Oxford III-V ICP-RIE
* [[ICP-RIE: III-V, Metal & Silicon Etcher|Oxford III-V ICP-RIE]]
* [https://lab.kni.caltech.edu/XeF2_Etcher_for_Silicon XeF2 Etcher]
* [https://lab.kni.caltech.edu/XeF2_Etcher_for_Silicon XeF2 Etcher]
* [https://lab.kni.caltech.edu/Plasma-Enhanced_Chemical_Vapor_Deposition_(PECVD) Oxford PECVD]
* [https://lab.kni.caltech.edu/Plasma-Enhanced_Chemical_Vapor_Deposition_(PECVD) Oxford PECVD]
* [https://lab.kni.caltech.edu/FlexAL_II:_Atomic_Layer_Deposition_(ALD) Oxford ALD]
* [https://lab.kni.caltech.edu/FlexAL_II:_Atomic_Layer_Deposition_(ALD) Oxford ALD]

Latest revision as of 19:13, 21 October 2026

Cobra III-V Etcher with ALE
Instrument Type Etching
Techniques III-V Semiconductor Etching
Atomic Layer Etching
Staff Manager Kelly McKenzie
Staff Email kmmckenz@caltech.edu
Staff Phone 626-395-5732
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235 Steele
Lab Phone 626-395-1532
Manufacturer Oxford Instruments
Model PlasmaPro 100 Cobra

Description

The Cobra inductively-coupled plasma reactive-ion etcher (ICP-RIE) with ALE is an Oxford Instruments Plasma Technology PlasmaPro 100 Cobra 300 system that is optimized for the etching of compound semiconductors and also features an ALE gas dose kit. In addition to a wide range of gases for etching a variety of III-V materials, this system is also configured with an atomic layer etching gas dose kit enabling controlled pulses of gas doses down to 10ms over a table temperature range of -150 to 400 °C. The system is also available for etching of more novel optical materials such as lithium niobate. This system supports wafer sizes up to 6 inches.

Applications
  • III-V material etch
  • Lithium niobate etch
  • Atomic layer etch
Allowed Material in Etcher
  • Etch materials: Si, SixNy, SiO2, Ge, InP, GaAs, GaN, Nb, Ta, LiNbO3, YVO4, MgB2, BaTiO3
  • Masks: PMMA/ZEP/SPR/AZ/maN resists, SiO2/Al2O3, Cr hard masks
  • Other: Metal in etch stack (not exposed to plasma)
Etching Gas List
  • SF6
  • O2
  • Ar
  • Cl2
  • BCl3
  • CH4
  • H2
  • HBr
  • SiCl4

Resources

SOPs & Troubleshooting
Process Documents
Review Articles
Manufacturer Manuals

Specifications

System Features
  • Process module frame and separate control rack that house the electronic sub systems, control units, pneumatics, and turbomolecular pump
  • PTIQ operating system
  • ICP process chamber with 200 mm pumping port, view port and end-point-detection port
  • 240 mm Cryo RIE electrode
  • 100-mTorr, temperature-stabilized capacitance manometer for process control with an active penning gauge for base pressure measurement
  • 200 mm pumping port is fitted with a 200 mm variable gate valve for chamber isolation and process pressure control
  • Twelve line gas pod with four non-toxic and six toxic digital mass-flow-controlled gas lines
  • Adixen ATH1600MT turbo pump backed by Pfeiffer A124H ELT dry pump
  • Single-wafer automatic insertion load lock with wafer presence sensor
  • Verity SD1024GH variable wavelength optical endpoint detection kit
System Specifications
  • Chamber wall heating 50 °C
  • Cryo table range -150 to 400 °C
  • ICP 300 mm remote high-density plasma source with 3 kW RF generator and automatic matching unit
  • Substrate bias control by 600 W RIE source with low power bias kit to allow accurate control <30 W
  • ALE gas dose kit enabling controlled, reproducible gas doses down to 10ms
  • Helium back-side wafer cooling and mechanical wafer clamping