== Description ==
The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).
The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV). <p>
It is important that users have the time needed to prepare their data and job files without the pressure of being on the clock. This approach gives them a better chance of not having to repeat charged exposures through so much trial and error. Please note that we do not charge for the time required to prepare pattern files (in Layout Beamer and Tracer), or for preparing exposure job files (cjob).  Users will receive instructions for secure remote access during training.
===== Operational Applications =====
===== Operational Applications =====
* Non-aligned electron beam lithography
* Non-aligned electron beam lithography
Line 28: Line 29:


== Resources ==
== Resources ==
===== Equipment Data =====
* [https://caltech.box.com/s/j19tuhv68bk0nsa5nruc95g4dizzxtr7 EBPG Pass-down equipment information]
===== General SOPs =====
===== General SOPs =====
* [https://caltech.box.com/s/y06o7wcnc336baqahj1z1qwuit3n0wm3 EBPG reservation and use policy (COVID-19 Phase 5 Updates)]
* [https://caltech.box.com/s/4lwz41kf9n7qpqxogsa7zl1kx55ldvj0 EBPG reservation and use policy (Updated June 2026)]
* [https://caltech.box.com/s/qzhf1h1su3a1vadl6p76mg6tav49uisn EBPG SOP]
* [https://caltech.box.com/s/qzhf1h1su3a1vadl6p76mg6tav49uisn EBPG SOP]
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/cwp88iw2q5t8eygl114zs8ywlhraxo16 EBPG reservation and use policy (Legacy version)]
* [https://caltech.box.com/s/cf5ix7iraea7m3jepjwylf4nd51d8hrg Remote EBPG access via HP Remote Graphics Server (Caltech-Only)]


===== Training Materials =====
===== Training Materials =====
Line 48: Line 44:


===== Sample Prep and Writing SOPs =====
===== Sample Prep and Writing SOPs =====
* [https://caltech.box.com/s/05w5x6u01gzpdn1ksa9r7967m2fdidai EBPG Handling Large Pattern Files SOP]
* [https://caltech.box.com/s/ys4qbxnsqfqbrdo4dm7t48z1z9dljuwi EBPG High Resolution Mode SOP]
* [https://caltech.box.com/s/ys4qbxnsqfqbrdo4dm7t48z1z9dljuwi EBPG High Resolution Mode SOP]
* [https://caltech.box.com/s/vpkguvtrdw9eup3rytljb5re9rfbe1fb EBPG 5200 Piece part prep SOP]
* [https://caltech.box.com/s/vpkguvtrdw9eup3rytljb5re9rfbe1fb EBPG 5200 Piece part prep SOP]
* [https://caltech.box.com/s/1vul3cyoudr1k3e8zoctne3oyt4irx3y EBPG 5200 Holder 200 SOP]
* [https://caltech.box.com/s/1vul3cyoudr1k3e8zoctne3oyt4irx3y EBPG 5200 Holder 200 SOP]
* [https://caltech.box.com/s/6yp4eq33y84y12hon075sbh1t7uukvay EBPG Preparing sample for exposure SOP]
* [https://caltech.box.com/s/6yp4eq33y84y12hon075sbh1t7uukvay EBPG Preparing sample for exposure SOP]
* [https://caltech.box.com/s/rwhke2ck8539d3p9pfhgvu3f62uasfhq EBPG Holder Fixture handling SOP]
* [https://caltech.box.com/s/c5gz16zs97vcsnlayr5kj7zffnv9mq81 EBPG Beam Adjustment SOP]
* [https://caltech.box.com/s/c5gz16zs97vcsnlayr5kj7zffnv9mq81 EBPG Beam Adjustment SOP]
* [https://caltech.box.com/s/3cs4x9gw0b3jdrg1acpt9e0lt5wbphzb EBPG Adjust Aperture SOP]
* [https://caltech.box.com/s/3cs4x9gw0b3jdrg1acpt9e0lt5wbphzb EBPG Adjust Aperture SOP]
Line 60: Line 58:
* [https://caltech.box.com/s/weqpi9oam0hbvxefqp8md1q4z8q14hze EBPG 5200 Secondary Electron Detector SOP]
* [https://caltech.box.com/s/weqpi9oam0hbvxefqp8md1q4z8q14hze EBPG 5200 Secondary Electron Detector SOP]
* [https://caltech.box.com/s/k2sicwqfbin5ktns5m30ir8wtdjqhea0 EBPG Holderfix SOP]
* [https://caltech.box.com/s/k2sicwqfbin5ktns5m30ir8wtdjqhea0 EBPG Holderfix SOP]
* [https://labrunr.caltech.edu/Equipment_2.aspx EBPG Remote Access SOP] (log into ''LabRunr'' and download SOP from EBPG 5200 page)


===== Advanced Troubleshooting SOPs =====
===== Advanced Troubleshooting SOPs =====
Line 84: Line 81:
* [https://caltech.box.com/s/ef3zou8b9xk597jxs7bs1s1yck1lo5cu App Note: Writing Time Optimization (Caltech-only access)]
* [https://caltech.box.com/s/ef3zou8b9xk597jxs7bs1s1yck1lo5cu App Note: Writing Time Optimization (Caltech-only access)]
* [https://caltech.box.com/s/c8hsz4opsgb0j8nmqq48v64wnlxth5l5 App Note: Formulas in Beamer Modules (Caltech-only access)]
* [https://caltech.box.com/s/c8hsz4opsgb0j8nmqq48v64wnlxth5l5 App Note: Formulas in Beamer Modules (Caltech-only access)]
* [https://caltech.box.com/s/wnx3fid41baefile9epmm797tbf81z59 App Note: Multipass (Caltech-only access)]
* [https://caltech.box.com/s/g3haulnez2ls6r2ezklcjei7jl8nx03b App Note: Multipass Exposure (Caltech-only access)]
* [https://caltech.box.com/s/yh1ku02vjnf3ew8uvmjbyn8hv5t0em72 App Note: Mixed Export Options (Caltech-only access)]
* [https://caltech.box.com/s/yh1ku02vjnf3ew8uvmjbyn8hv5t0em72 App Note: Mixed Export Options (Caltech-only access)]
* [https://caltech.box.com/s/9wbovly55qu2plfmoian6a7ocbw7pk2h App Note: GPF Formatter (Caltech-only access)]
* [https://caltech.box.com/s/9wbovly55qu2plfmoian6a7ocbw7pk2h App Note: GPF Formatter (Caltech-only access)]
* [https://www.genisys-gmbh.com/webinar-series-beamer-training.html Webinar Series - BEAMER Training]
* [https://www.genisys-gmbh.com/webinar-series-proximity-effect-in-e-beam-lithography.html Webinar Series: Proximity Effect in E-Beam Lithography]
* [https://www.genisys-gmbh.com/webinar-e-beam-lithography-simulation.html Webinar: e-Beam Lithography Simulation]
* [https://caltech.box.com/s/iaq5dsl4olmj1er5gfm805hfpy4gknk9 March 2020 Genisys BEAMeeting at Caltech]
* [https://caltech.box.com/s/iaq5dsl4olmj1er5gfm805hfpy4gknk9 March 2020 Genisys BEAMeeting at Caltech]
* [https://caltech.box.com/s/uwlcuus2wny3hoplvszazhxgb6fzzzwq June 2020 Genisys BEAMeeting Layout Beamer training video (Caltech-only access)]
* [https://caltech.box.com/s/uwlcuus2wny3hoplvszazhxgb6fzzzwq June 2020 Genisys BEAMeeting Layout Beamer training video (Caltech-only access)]
Line 104: Line 104:
* [https://caltech.box.com/s/ji4zqki1wps2anyjy45on7cp0szvb3yk Supramolecular Resist processing (Caltech-only access)]
* [https://caltech.box.com/s/ji4zqki1wps2anyjy45on7cp0szvb3yk Supramolecular Resist processing (Caltech-only access)]
* [https://caltech.box.com/s/jsetuvrq4ec1alqvn25pz11kmtzuw8rc Laurell Spinner cleaning SOP]
* [https://caltech.box.com/s/jsetuvrq4ec1alqvn25pz11kmtzuw8rc Laurell Spinner cleaning SOP]
* [https://caltech.box.com/s/ybozdh0es8nzd6ujlx28lk7cnimlxwfm New Laurell Spinner WS-650Mz-23NPPB-IND Documentation (Caltech-only access)]


===== Manufacturer Manuals =====
===== Manufacturer Manuals =====
Line 112: Line 113:
* [https://caltech.box.com/s/e177zgemo96fddfrkdqsh3cu15k0snbg CEBUS 2021 Presentations (Caltech-only access)]
* [https://caltech.box.com/s/e177zgemo96fddfrkdqsh3cu15k0snbg CEBUS 2021 Presentations (Caltech-only access)]
* [https://labrunr.caltech.edu/Equipment_2.aspx Laurell Spin Coater Manual] (log into ''LabRunr'' and download Manual from EBPG 5000+ page)
* [https://labrunr.caltech.edu/Equipment_2.aspx Laurell Spin Coater Manual] (log into ''LabRunr'' and download Manual from EBPG 5000+ page)
* [https://caltech.box.com/s/7gw32ios7yqj3d8ghj336u0ksm6gued6 Torrey Pines HS30A Programmable hotplate manual]


== Specifications ==
== Specifications ==
Line 127: Line 129:
* [[EBPG 5000+: 100 kV Electron Beam Lithography | EBPG 5000+: 100 kV Electron Beam Lithography]]
* [[EBPG 5000+: 100 kV Electron Beam Lithography | EBPG 5000+: 100 kV Electron Beam Lithography]]
* [[Quanta 200F: SEM, ESEM, Lithography & Probe Station | Quanta 200F: SEM with 1-30 kV Electron Beam Lithography]]
* [[Quanta 200F: SEM, ESEM, Lithography & Probe Station | Quanta 200F: SEM with 1-30 kV Electron Beam Lithography]]
* [[Tecnai TF-20: 200 kV TEM, STEM, EDS, EELS, EFTEM & Lithography | Tecnai TF-20: TEM & STEM with 80-200 kV Electron Beam Lithography]]
<!---* [[Tecnai TF-20: 200 kV TEM, STEM, EDS, EELS, EFTEM & Lithography | Tecnai TF-20: TEM & STEM with 80-200 kV Electron Beam Lithography]]--->
===== Ion Beam Lithography =====
===== Ion Beam Lithography =====
* [[ORION NanoFab: Helium, Neon & Gallium FIB | ORION NanoFab: Helium (5-40 kV), Neon (5-35 kV) & Gallium (1-30 kV) Focused Ion Beam Lithography & Microscopy]]
* [[ORION NanoFab: Helium, Neon & Gallium FIB | ORION NanoFab: Helium (5-40 kV), Neon (5-35 kV) & Gallium (1-30 kV) Focused Ion Beam Lithography & Microscopy]]

Latest revision as of 16:18, 7 August 2026

EBPG 5200
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5200

Description

The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

It is important that users have the time needed to prepare their data and job files without the pressure of being on the clock. This approach gives them a better chance of not having to repeat charged exposures through so much trial and error. Please note that we do not charge for the time required to prepare pattern files (in Layout Beamer and Tracer), or for preparing exposure job files (cjob). Users will receive instructions for secure remote access during training.

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

General SOPs
Training Materials
Sample Prep and Writing SOPs
Advanced Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 200 μm, 300 μm, 400 μm



Electron Beam Lithography