===== Applications ===== | ===== Applications ===== | ||
* Metal deposition (Ti, Pt, Au, Al) | * Metal deposition (Ti, Pt, Au, Al) | ||
** Other materials may be available upon request with restrictions: metals such as Cr, Fe, Ni, Co are not available. If you wish to deposit these see the links to related systems on this page. | |||
* Lift-off | * Lift-off | ||
* Non-selective etch | * Non-selective etch | ||
| Line 26: | Line 27: | ||
== Resources == | == Resources == | ||
===== SOPs & Troubleshooting ===== | ===== SOPs & Troubleshooting ===== | ||
* [https://caltech.box.com/s/9sx2vhd9gz5rdhviexii8hj6lftvxguy KNI SOP] | * [https://caltech.box.com/s/9sx2vhd9gz5rdhviexii8hj6lftvxguy KNI SOP] | ||
| Line 46: | Line 45: | ||
===== Video Tutorials ===== | ===== Video Tutorials ===== | ||
* [https://youtu.be/jq5M7fkgpfM Labline Training] | * [https://youtu.be/jq5M7fkgpfM Labline Training] | ||
* [https://youtu.be/5C6It9YO_jg Sample Load & Transfer] | |||
== Specifications == | == Specifications == | ||
| Line 54: | Line 54: | ||
* Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source | * Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source | ||
* 1x Argon ion source (Filament type) | * 1x Argon ion source (Filament type) | ||
* Accepts up to 1x 150mm wafer or smaller wafers/pieces | |||
== Related Instrumentation in the KNI == | == Related Instrumentation in the KNI == | ||
| Line 61: | Line 62: | ||
===== Electron Beam Evaporation Systems ===== | ===== Electron Beam Evaporation Systems ===== | ||
* [[ | * [[AJA Orion ATC Series Electron Beam Evaporator|AJA Orion ATC Series Electron Beam Evaporator]] | ||
===== Chemical Vapor Deposition ===== | ===== Chemical Vapor Deposition ===== | ||
* [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]] | * [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]] | ||
* [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]] | * [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]] | ||
Latest revision as of 19:27, 19 March 2026
|
Description
The Labline electron beam evaporator system is a load-locked platform with a cryopump for fast sample turnaround and a user-friendly interface for precise control of film parameters during deposition. It is fitted with a Kaufman and Robinson EH 400 End-Hall permanent magnet ion source that can be used for cleaning substrates and ion-assisted deposition during evaporation.
Applications
- Metal deposition (Ti, Pt, Au, Al)
- Other materials may be available upon request with restrictions: metals such as Cr, Fe, Ni, Co are not available. If you wish to deposit these see the links to related systems on this page.
- Lift-off
- Non-selective etch
- Ion-assisted deposition (simultaneous etching & deposition)
Resources
SOPs & Troubleshooting
Tool Reservation Rules
| Advanced Reservation (days) | Limit per Reservation (hrs) | Limit per week (hrs) | |
|---|---|---|---|
| Weekday | 7 | 6 | 18 |
| Weeknight | 7 | 8 | 18 |
| Weekend | 7 | 12 | 18 |
Video Tutorials
Specifications
Hardware Specifications
- Typical base pressure: 1E-7 to 1E-8 Torr
- All dry pumping system (cryo & scroll pumps)
- Load-lock-equipped system with manual wafer transfer
- Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
- 1x Argon ion source (Filament type)
- Accepts up to 1x 150mm wafer or smaller wafers/pieces