Labline: Electron Beam Evaporator: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Alexw (talk | contribs)
No edit summary
Alexw (talk | contribs)
 
(8 intermediate revisions by 4 users not shown)
Line 13: Line 13:
|Model = Labline
|Model = Labline
|Techniques = E-beam Evaporation,<br>Ion-Assisted Deposition (IAD),</br>Ion Milling
|Techniques = E-beam Evaporation,<br>Ion-Assisted Deposition (IAD),</br>Ion Milling
|EmailList = kni-labline@caltech.edu
|EmailList = kni-labline
|EmailListName =  Labline
|EmailListName =  Labline
}}
}}
Line 21: Line 21:
===== Applications =====
===== Applications =====
* Metal deposition (Ti, Pt, Au, Al)
* Metal deposition (Ti, Pt, Au, Al)
** Other materials may be available upon request with restrictions: metals such as Cr, Fe, Ni, Co are not available. If you wish to deposit these see the links to related systems on this page.
* Lift-off
* Lift-off
* Non-selective etch
* Non-selective etch
Line 29: Line 30:
* [https://caltech.box.com/s/9sx2vhd9gz5rdhviexii8hj6lftvxguy KNI SOP]
* [https://caltech.box.com/s/9sx2vhd9gz5rdhviexii8hj6lftvxguy KNI SOP]
* [https://caltech.box.com/s/sqfi1s85wykxzecvt0mqdv5fr27nggvc Troubleshooting Guide]
* [https://caltech.box.com/s/sqfi1s85wykxzecvt0mqdv5fr27nggvc Troubleshooting Guide]
=== Tool Reservation Rules ===
{| class="wikitable"
|-
!  !! Advanced Reservation (days) !! Limit per Reservation (hrs) !! Limit per week (hrs)
|-
| Weekday || 7 || 6 || 18
|-
| Weeknight || 7 || 8 || 18
|-
| Weekend || 7 || 12 || 18
|}


===== Video Tutorials =====
===== Video Tutorials =====
* [https://youtu.be/jq5M7fkgpfM Labline Training]
* [https://youtu.be/jq5M7fkgpfM Labline Training]
* [https://youtu.be/5C6It9YO_jg Sample Load & Transfer]


== Specifications ==
== Specifications ==
Line 40: Line 54:
* Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
* Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
* 1x Argon ion source (Filament type)
* 1x Argon ion source (Filament type)
* Accepts up to 1x 150mm wafer or smaller wafers/pieces


== Related Instrumentation in the KNI ==
== Related Instrumentation in the KNI ==
Line 47: Line 62:


===== Electron Beam Evaporation Systems =====
===== Electron Beam Evaporation Systems =====
* [[CHA: Electron Beam Evaporator|CHA: Electron Beam Evaporator]]
* [[AJA Orion ATC Series Electron Beam Evaporator|AJA Orion ATC Series Electron Beam Evaporator]]


===== Chemical Vapor Deposition =====
===== Chemical Vapor Deposition =====
* [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]]
* [[FlexAL II: Atomic Layer Deposition (ALD)|FlexAL II: Atomic Layer Deposition (ALD)]]
* [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]]
* [[Plasma-Enhanced Chemical Vapor Deposition (PECVD)|Plasma-Enhanced Chemical Vapor Deposition (PECVD)]]

Latest revision as of 19:27, 19 March 2026

Labline Evaporator
Instrument Type Deposition
Techniques E-beam Evaporation,
Ion-Assisted Deposition (IAD),
Ion Milling
Staff Manager Alex Wertheim
Staff Email alexw@caltech.edu
Staff Phone 626-395-3371
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235C Steele
Lab Phone 626-395-1539
Manufacturer Kurt J. Lesker Company
Model Labline

Description

The Labline electron beam evaporator system is a load-locked platform with a cryopump for fast sample turnaround and a user-friendly interface for precise control of film parameters during deposition. It is fitted with a Kaufman and Robinson EH 400 End-Hall permanent magnet ion source that can be used for cleaning substrates and ion-assisted deposition during evaporation.

Applications
  • Metal deposition (Ti, Pt, Au, Al)
    • Other materials may be available upon request with restrictions: metals such as Cr, Fe, Ni, Co are not available. If you wish to deposit these see the links to related systems on this page.
  • Lift-off
  • Non-selective etch
  • Ion-assisted deposition (simultaneous etching & deposition)

Resources

SOPs & Troubleshooting

Tool Reservation Rules

Advanced Reservation (days) Limit per Reservation (hrs) Limit per week (hrs)
Weekday 7 6 18
Weeknight 7 8 18
Weekend 7 12 18
Video Tutorials

Specifications

Hardware Specifications
  • Typical base pressure: 1E-7 to 1E-8 Torr
  • All dry pumping system (cryo & scroll pumps)
  • Load-lock-equipped system with manual wafer transfer
  • Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
  • 1x Argon ion source (Filament type)
  • Accepts up to 1x 150mm wafer or smaller wafers/pieces
Sputtering Systems
Electron Beam Evaporation Systems
Chemical Vapor Deposition