Full Service Rates: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
No edit summary
No edit summary
 
(6 intermediate revisions by the same user not shown)
Line 1: Line 1:
The KNI Laboratory offers full-service work for internal (Caltech/JPL) customers as well as external customers from industry, government, and academia. We welcome electron beam lithography requests, in addition to other device fabrication needs. Full-service work is project dependent on staff availability, timeline, and scope, and will be reviewed by KNI technical staff. This page covers the pricing for external full-service customers. KNI offers no guarantees for the end product.
The KNI Laboratory offers full-service work for internal (Caltech/JPL) customers as well as external customers from industry, government, and academia. We welcome electron beam lithography requests, in addition to other device fabrication needs. Full-service work is project dependent based on staff availability, timeline, and scope, and will be reviewed by KNI technical staff. Full-service work is best for one-off project needs. Ongoing device fab work is typically outside our capacity. This page covers the pricing for '''external''' full-service customers. '''Note:''' Internal customers (Caltech/JPL) interested in full-service work: review the details [[Usage Rates|'''here''']]. KNI offers no guarantees for the end product.  
 
'''Note:''' Internal customers (Caltech/JPL) interested in full-service work: review the details [[Usage Rates|'''here''']].


=== Why KNI? ===
=== Why KNI? ===
Line 19: Line 17:
* '''Mask fabrication''' — photomask writing for optical lithography step-and-repeat
* '''Mask fabrication''' — photomask writing for optical lithography step-and-repeat


=== '''Cost''' ===
=== Electron Beam Lithography Specifications ===
The prices below are for industry customers (for-profit entities). If you are a non-Caltech academic or government customer, please contact us for the rates. Rates are effective October 1, 2025.
{| class="wikitable"
|+
|'''Accelerating Voltage'''
|20/50/100 kV (normally operated at 100 kV)
|-
|'''Current Range'''
|50 pA - 200 nA
|-
|'''Resolution'''
|Sub-10 nm
|-
|'''Main Field Size'''
|<nowiki>Up to 1 mm x 1 mm | 20-bit DAC</nowiki>
|-
|'''Max. Writing Frequency'''
|100 MHz
|-
|'''Aperture Sizes'''
|200, 300, and 400 µm (selection varies by system)
|-
|'''Substrate Handling'''
|Piece parts (few mm to wafer scale), wafers up to 6", mask plates up to 6" ; 5200 expandable to 200 mm
|-
|'''Writing Modes'''
|Non-aligned & aligned (direct-write) electron beam lithography
|-
|'''Data Preparation'''
|GenISys Layout BEAMER & TRACER
|}
 
=== Cost ===
The prices below are for industry customers (for-profit entities). If you are a non-Caltech academic or government customer, please contact us for the rates. Rates are effective October 1, 2026.
{| class="wikitable"
{| class="wikitable"
|'''Resource'''
|'''Resource'''
Line 26: Line 55:
|-
|-
|Technical Staff Effort  
|Technical Staff Effort  
|$                                             200.00
|$                                             170.00
|-
|-
|EBPG 5000+ or 5200
|EBPG 5000+ or 5200
|$                                             442.00
|$                                             455.00
|-
|-
|Nova 600 FIB
|Nova 600 FIB
|$                                             255.00
|$                                             263.00
|-
|-
|III-V Cobra ALE Etcher
|III-V Cobra ALE Etcher
|$                                             204.00
|$                                             210.00
|-
|-
|PlasmaPro PECVD (oxide, nitride)
|PlasmaPro PECVD (oxide, nitride)
|$                                             204.00
|$                                             210.00
|-
|-
|FlexAL II ALD/ALE
|FlexAL II ALD/ALE
Line 44: Line 73:
|-
|-
|Legacy PlasmaLab PECVD (silicon)
|Legacy PlasmaLab PECVD (silicon)
|$                                             136.00
|$                                             140.00
|-
|-
|Legacy Oxford Etchers (DRIE, III-V, Dielectric)
|Legacy Oxford Etchers (DRIE, III-V, Dielectric)
|$                                             136.00
|$                                             140.00
|-
|-
|Nanoscribe PPGT (2D/3D print)
|Nanoscribe PPGT (2D/3D print)
|$                                              17.00
|$                                              27.00
|-
|-
|Administrative Fee (per transaction)
|Administrative Fee (per transaction)
|$                                             340.00
|$                                             170.00
|}
|}
'''''Note:''' The prices shown here include Caltech's indirect cost rate.''  
'''''Note:''' The prices shown here include Caltech's indirect cost rate.''  


=== '''To get started''' ===
=== How to Get Started ===
Send an email with your project description and timeline needs to [mailto:kni@caltech.edu kni@caltech.edu]. We will review the request and send a price estimate based on the information provided. We require a purchase order to initiate the full-service work.
Send an email with your project description and timeline needs to [mailto:kni@caltech.edu kni@caltech.edu]. We will review the request and send a price estimate based on the information provided. We require a purchase order to initiate the full-service work.

Latest revision as of 22:11, 29 October 2026

The KNI Laboratory offers full-service work for internal (Caltech/JPL) customers as well as external customers from industry, government, and academia. We welcome electron beam lithography requests, in addition to other device fabrication needs. Full-service work is project dependent based on staff availability, timeline, and scope, and will be reviewed by KNI technical staff. Full-service work is best for one-off project needs. Ongoing device fab work is typically outside our capacity. This page covers the pricing for external full-service customers. Note: Internal customers (Caltech/JPL) interested in full-service work: review the details here. KNI offers no guarantees for the end product.

Why KNI?

  • Full process flows: resist coating through etch/deposition to final device, under one roof
  • Experienced staff: fill-time expert engineers managing tools daily
  • Caltech ecosystem: proximity to world-class research in photonics, quantum, and materials
  • IP-secure: NDA option to protect ownership and inventorship rights

Application Areas

  • Quantum devices — superconducting qubits, ion trap electrodes, single-photon sources
  • Photonic integrated circuits — waveguides, grating couplers, ring resonators, metasurfaces
  • AR/VR optics — diffractive waveguide masters, surface-relief gratings, metalenses
  • RF & III-V devices — HEMT gates, fine-pitch test structures, GaAs/GaN/InP
  • Sensors & MEMS — IR detectors, nanoelectromechanical systems, biomedical devices
  • Mask fabrication — photomask writing for optical lithography step-and-repeat

Electron Beam Lithography Specifications

Accelerating Voltage 20/50/100 kV (normally operated at 100 kV)
Current Range 50 pA - 200 nA
Resolution Sub-10 nm
Main Field Size Up to 1 mm x 1 mm | 20-bit DAC
Max. Writing Frequency 100 MHz
Aperture Sizes 200, 300, and 400 µm (selection varies by system)
Substrate Handling Piece parts (few mm to wafer scale), wafers up to 6", mask plates up to 6" ; 5200 expandable to 200 mm
Writing Modes Non-aligned & aligned (direct-write) electron beam lithography
Data Preparation GenISys Layout BEAMER & TRACER

Cost

The prices below are for industry customers (for-profit entities). If you are a non-Caltech academic or government customer, please contact us for the rates. Rates are effective October 1, 2026.

Resource Hourly Rate (excluding admin fee)
Technical Staff Effort $                                             170.00
EBPG 5000+ or 5200 $                                             455.00
Nova 600 FIB $                                             263.00
III-V Cobra ALE Etcher $                                             210.00
PlasmaPro PECVD (oxide, nitride) $                                             210.00
FlexAL II ALD/ALE $                                             170.00
Legacy PlasmaLab PECVD (silicon) $                                             140.00
Legacy Oxford Etchers (DRIE, III-V, Dielectric) $                                             140.00
Nanoscribe PPGT (2D/3D print) $                                             27.00
Administrative Fee (per transaction) $                                             170.00

Note: The prices shown here include Caltech's indirect cost rate.

How to Get Started

Send an email with your project description and timeline needs to kni@caltech.edu. We will review the request and send a price estimate based on the information provided. We require a purchase order to initiate the full-service work.