EBPG 5200: 100 kV Electron Beam Lithography: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
Derose (talk | contribs)
Derose (talk | contribs)
 
(One intermediate revision by the same user not shown)
Line 34: Line 34:
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/jq0s85sdsd069cv9aesdfixy5fueihyh User's Guide to the EBPG pg computer desktop]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/9whswv26y0w6yua8073nw080r3lcfdz4 EBPG Troubleshooting Guide]
* [https://caltech.box.com/s/cf5ix7iraea7m3jepjwylf4nd51d8hrg Remote EBPG access via HP Remote Graphics Server (Caltech-Only)]


===== Training Materials =====
===== Training Materials =====
Line 59: Line 58:
* [https://caltech.box.com/s/weqpi9oam0hbvxefqp8md1q4z8q14hze EBPG 5200 Secondary Electron Detector SOP]
* [https://caltech.box.com/s/weqpi9oam0hbvxefqp8md1q4z8q14hze EBPG 5200 Secondary Electron Detector SOP]
* [https://caltech.box.com/s/k2sicwqfbin5ktns5m30ir8wtdjqhea0 EBPG Holderfix SOP]
* [https://caltech.box.com/s/k2sicwqfbin5ktns5m30ir8wtdjqhea0 EBPG Holderfix SOP]
* [https://labrunr.caltech.edu/Equipment_2.aspx EBPG Remote Access SOP] (log into ''LabRunr'' and download SOP from EBPG 5200 page)


===== Advanced Troubleshooting SOPs =====
===== Advanced Troubleshooting SOPs =====

Latest revision as of 16:18, 7 August 2026

EBPG 5200
Instrument Type Lithography
Techniques Electron Beam Lithography
Staff Manager Guy A. DeRose, PhD
Staff Email derose@caltech.edu
Staff Phone 626-395-3423
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B233C Steele
Lab Phone 626-395-1531 & -1540
Manufacturer Raith Lithography BV
Model EBPG 5200

Description

The Raith EBPG 5200 is a dedicated direct-write Electron Beam Pattern Generator that is used to pattern large areas by high-resolution electron beam lithography. This instrument has substrate holders to handle 3" wafers, piece parts from a couple of mm to 3" diameter and up to 6.35 mm thick, and 6" mask plates. This instrument can be outfitted with substrate holders to handle up to 200 mm wafers. While this instrument can be set to operate at 20, 50, or 100 keV, it is normally set for 100 keV operation (i.e. with an accelerating voltage of 100 kV, the average energy per electron is 100 keV).

It is important that users have the time needed to prepare their data and job files without the pressure of being on the clock. This approach gives them a better chance of not having to repeat charged exposures through so much trial and error. Please note that we do not charge for the time required to prepare pattern files (in Layout Beamer and Tracer), or for preparing exposure job files (cjob). Users will receive instructions for secure remote access during training.

Operational Applications
  • Non-aligned electron beam lithography
  • Aligned (aka direct-write) electron beam lithography
Scientific / Technical Applications
  • Nanophotonics
  • Nano-optics
  • Waveguides

Resources

General SOPs
Training Materials
Sample Prep and Writing SOPs
Advanced Troubleshooting SOPs
Data Preparation Resources
Lithography Process Information
Manufacturer Manuals

Specifications

  • Voltage Range: 20, 50 or 100 kV
  • Current Range: 50 pA to 200 nA
  • Main Field Size: Up to 1 mm x 1 mm
  • Main Field Resolution: 20 bit
  • Maximum Writing Frequency: 100 MHz
  • Aperture Sizes: 200 μm, 300 μm, 400 μm



Electron Beam Lithography
Ion Beam Lithography