Parylene Coater: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
No edit summary |
||
| (4 intermediate revisions by 2 users not shown) | |||
| Line 7: | Line 7: | ||
|RoomLocation = B203 Steele | |RoomLocation = B203 Steele | ||
|LabPhone = 626-395-1539 | |LabPhone = 626-395-1539 | ||
|PrimaryStaff = [[ | |PrimaryStaff = [[Nathan S. Lee]] | ||
|StaffEmail = | |StaffEmail = nathslee@caltech.edu | ||
|StaffPhone = 626-395- | |StaffPhone = 626-395-4386 | ||
|Manufacturer = Para Tech | |Manufacturer = Para Tech | ||
|Model = LabTop 3000 | |Model = LabTop 3000 | ||
|Techniques = Parylene Deposition | |Techniques = Parylene Deposition | ||
|RequestTraining = | |RequestTraining = Alexw@caltech.edu | ||
|EmailList = kni-parylene | |EmailList = kni-parylene | ||
|EmailListName = Parylene | |EmailListName = Parylene | ||
}} | }} | ||
Latest revision as of 00:26, 16 July 2025
|
Description
The ParaTech LabTop 3000 Parylene coater uses a multi-stage thermal process to deposit a conformal parylene film on your substrates. Multiple wafers up to 150 mm diameter may be coated at once. Samples are under vacuum during and not subject to heat during coating.
Applications
- Bio-compatible/moisture protection packaging
- Dielectric polymer coating