XeF2 Etcher for Silicon: Difference between revisions

From the KNI Lab at Caltech
Jump to navigation Jump to search
mNo edit summary
No edit summary
 
(6 intermediate revisions by 4 users not shown)
Line 5: Line 5:
|ImageTwo =  
|ImageTwo =  
|InstrumentType = [[Equipment_List#Etching|Etching]]
|InstrumentType = [[Equipment_List#Etching|Etching]]
|RoomLocation =  
|RoomLocation = B235C Steele
|LabPhone = 626-395-1539
|LabPhone = 626-395-1539
|PrimaryStaff = [[Alex Wertheim]]
|PrimaryStaff = [[Kelly McKenzie]]
|StaffEmail = alexw@caltech.edu
|StaffEmail = kmmckenz@caltech.edu
|StaffPhone = 626-395-3371
|StaffPhone = 626-395-5732
|Manufacturer = N/A
|Manufacturer = N/A
|Model = N/A
|Model = N/A
|Techniques = Selective dry Si etching
|Techniques = Selective dry Si etching
|RequestTraining = alexw@caltech.edu
|RequestTraining = kmmckenz@caltech.edu
|EmailList = kni-XeF2@caltech.edu
|EmailList = kni-XeF2
|EmailListName = XeF<sub>2</sub>
|EmailListName = XeF<sub>2</sub>
}}
}}

Latest revision as of 19:17, 29 June 2024

XeF2 Silicon Etcher
XeF2-Etcher.jpg
Instrument Type Etching
Techniques Selective dry Si etching
Staff Manager Kelly McKenzie
Staff Email kmmckenz@caltech.edu
Staff Phone 626-395-5732
Reserve time on FBS
Request training via FBS User Dashboard
Lab Location B235C Steele
Lab Phone 626-395-1539
Manufacturer N/A
Model N/A

Description

The XeF2 etcher flows pressure- and time-controlled pulses of XeF2 gas into a chamber to deliver an isotropic etch that is highly selective only to silicon. It is commonly used to remove Si under layers that are accessed through vias, in order to suspend membranes and other structures in MEMS devices.

Applications
  • Very high selectivity dry Si etching
  • MEMS fabrication

Resources

SOPs