Description
Machines of this series bond aluminum or gold wires, ranging from 0.0007 to 0.0020 inches in diameter, by the wedge-wedge technique. Ultrasonic energy is used to attach aluminum wire at room temperature, while adding work piece heat is used for attaching gold wire. Wire-bonding is often one of the last steps in the device fabrication process.
Applications
- Bonding aluminum wire to a metal bond pad