Labline: Electron Beam Evaporator: Difference between revisions
Jump to navigation
Jump to search
No edit summary |
mNo edit summary |
||
Line 5: | Line 5: | ||
|ImageTwo = | |ImageTwo = | ||
|InstrumentType = [[Equipment_List#Deposition|Deposition]] | |InstrumentType = [[Equipment_List#Deposition|Deposition]] | ||
|RoomLocation = | |RoomLocation = B235C Steele | ||
|LabPhone = 626-395-1539 | |LabPhone = 626-395-1539 | ||
|PrimaryStaff = [[Alex Wertheim]] | |PrimaryStaff = [[Alex Wertheim]] |
Revision as of 21:10, 27 May 2019
|
Description
The Labline electron beam evaporator system is a load-locked platform with a cryopump for fast sample turnaround and a user-friendly interface for precise control of film parameters during deposition. It is fitted with a Kaufman and Robinson EH 400 End-Hall permanent magnet ion source that can be used for cleaning substrates and ion-assisted deposition during evaporation.
Applications
- Metal deposition (Ti, Pt, Au, Al)
- Lift-off
- Non-selective etch
- Ion-assisted deposition (simultaneous etching & deposition)
Resources
SOPs & Troubleshooting
Video Tutorials
Specifications
Hardware Specifications
- Typical base pressure: 1E-7 to 1E-8 Torr
- All dry pumping system (cryo & scroll pumps)
- Load-lock-equipped system with manual wafer transfer
- Evaporation Source: 1x single emitter, 4-pocket e-beam evaporation source
- 1x Argon ion source (Filament type)